Added a PEI plate for my Artillery Genius using bull clips, and after leveling the leveling/adhesion test print comes out like this. Is this just me leveling the bed too close to the nozzle, or is it the pei plate not heating up as much as the original glass bed? It’s at 60c btw

  • jokeyrhyme@lemmy.ml
    link
    fedilink
    English
    arrow-up
    1
    ·
    3 days ago

    slightly off topic:

    do you have the bed start at e.g. 60 for the first layer and then 65 for subsequent layers?

    does raising the temperature mid print like this help with warping or something?

    • Jaeger86@lemmy.world
      link
      fedilink
      English
      arrow-up
      1
      ·
      edit-2
      2 days ago

      I start at 62(and stay there) that’s the magic number i found for my sovol 6 and 6 plus, at lower I would experience warping and bad bed adhesion. And I’ve had the same correlation with mine at home and the 3 I have at work